YDT757 Galvanized Coating Adhesion Hammer Drop Test Device
Product details:ZLT-BC4
To test Adhesion of hot dip galvanized coatings,according to YDT 757 Annex C,BS 729 clause 7.
Test principle:drop freely impact samples of the hammer head to test galvanized layer meets standards or not.
Standard Outfit:
1 hammer weight,of 210g±1g,by 45# steel,hardness HS ≥40.
1 solid oak,wight of 70g,
1 steel base,15mm thick,250mm long,250mm wide.